The silica added to the furnace charge behaves as a strong acid at a high temperature, about 1500°C, and combines with the calcium constituent of the phosphate rock to form calcium silicate ( Schipper et al, 2001; Joseph, 2008;Mark, 2011 In the second stage, the elemental phosphorus is oxidized with air to become phosphorous pentaoxide (P 2 O